| Sign In | Join Free | My insurersguide.com |
|
| Categories | Studded Tube |
|---|---|
| Brand Name: | YUHONG |
| Certification: | ABS, BV, ISO, ASTM, SGS |
| Place of Origin: | China |
| MOQ: | 200-500KGS |
| Price: | Negotiable |
| Payment Terms: | L/C,T/T,AT SIGHT |
| Supply Ability: | According to Clients' requirements |
| Delivery Time: | 45-75 Days (Depend on Customer's Requirement |
| Packaging Details: | Ply-wooden Cases with Steel Frames(both ends of pipes have plastic caps) |
| Bare Tube Diameter: | 25-219mm |
| Fin Pitch: | 8-30mm |
| Fin Height: | 5-35mm |
| Fin Thick: | Φ5-20mm |
| Application: | Heat Exchangers, Refinery Air Cooler, Heater, Cooling tower |
| Base Tube Specification & Material:: | ASTM A213 T9 |
| Company Info. |
| YUHONG HOLDING GROUP CO., LTD |
| Verified Supplier |
| View Contact Details |
| Product List |
ASTM A213 T9 Studded Fin Tube is a high-temperature heat transfer component engineered for extreme thermal and corrosive service. It consists of a seamless chromium-molybdenum alloy steel base tube (ASTM A213 T9) with stud-type fins resistance-welded perpendicularly to the surface. This robust construction maximizes heat flux in high-ash/flue gas environments (up to 600°C/1,112°F), offering superior oxidation resistance and 3x longer life than carbon steel tubes in waste heat boilers, reformers, and fired heaters.
Element | Content (%) | Critical Function |
Chromium (Cr) | 8.0–10.0 | Oxidation resistance |
Molybdenum (Mo) | 0.90–1.10 | High-temp strength |
Carbon (C) | 0.15 max | Weldability |
Manganese (Mn) | 0.30–0.60 | Toughness |
Silicon (Si) | 0.25–1.00 | Deoxidation |
Phosphorus (P) | ≤ 0.025 | Purity |
Sulfur (S) | ≤ 0.025 | Ductility |
Mechanical Properties (System)
Property | Base Tube (T9) |
Tensile Strength | ≥ 415 MPa |
Yield Strength | ≥ 205 MPa |
Max Service Temp. | 600°C (1,112°F) |
Hardness | ≤ 179 HB |
Thermal Conductivity | 36.7 W/m·K |
· Refinery Heaters: Convection sections in CDU/VDU heaters (resists sulfidation).
· Chemical Reformers: Syngas coolers in methanol/ammonia plants.
· Waste Heat Recovery: Boilers in cement/steel mills (handles >80g/Nm³ fly ash).
· Power Generation: SCR system heat exchangers for coal-fired plants.
· Petrochemical: Cracking furnace convection tubes.
>4. >Why This Solution Dominates:
· 10-Year Lifespan: Withstands 650°C cyclic operation per NACE RP0492.
· Ash Erosion Resistance: Stud spacing blocks ash buildup – 40% lower fouling vs. helical
fins.
· Cost Saving: 35% lower OPEX than refractory-lined carbon steel tubes.
· Customization: Stud height (15–40mm), diameter (3–8mm), and pitch optimization.

|