| Sign In | Join Free | My insurersguide.com |
|
| Categories | High Temperature Alloy |
|---|---|
| Brand Name: | KAIXIN |
| Model Number: | KX-Alloy3039 |
| Certification: | ISO9001:2015 |
| Place of Origin: | China |
| MOQ: | 200KG |
| Price: | To negotiate |
| Payment Terms: | T/T, L/C |
| Supply Ability: | 50~80TONS per MONTH |
| Delivery Time: | 45~60days |
| Packaging Details: | Wooden Box, size as per guests request |
| Shape: | Wire, Strip, Rod, Tube, Plate |
| Alloy Type: | Single-phase Austenitic Solid Solution Reinforced Alloy |
| Raw Materials: | NI Rem,CR19-22% |
| Executive Standard: | ASTM |
| Delivery State: | Sosoloid |
| Application: | Aerospace components |
| Features: | Fatigue resistance, heat strength and oxidation resistance |
| Size: | Negotiable |
| Company Info. |
| Danyang Kaixin Alloy Material Co., Ltd. |
| Verified Supplier |
| View Contact Details |
| Product List |
KX ХН75МБГЮ(Russian) Light Rod Plate Structural Operating Temperature Range For High Temperature Alloy
Product Description and Application
ХН75МБГЮ(Russian) is also known as "KN602, shed osan 75 manas (Russia), and GH39.
ХН75МБГЮ(Russian) is a single-phase Austenitic solid solution reinforced alloy with moderate thermal strength and good thermal fatigue properties below 800℃ and good oxidation resistance below 1000℃. Long-term use with stable structure and has good cold formability and welding performance. It is suitable for aero engine combustion chamber and afterburner parts used for a long time below 850℃. The alloy can produce sheet, bar, wire, pipe and forgings.
Process Performance and Requirements
Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
| Grade | Ni | Cr | Fe | Mo | Nb | Co | C | Mn |
ХН75МБГЮ (Russian) | Rem | 19.0-22 | ≤3.0 | 1.8-2.3 | 0.9-1.3 | ≤0.08 | ≤0.4 | |
| Al | Ti | Si | P | S | Cu | |||
| 0.35-0.75 | 0.35-0.75 | ≤0.8 | ≤0.020 | ≤0.012 | ≤0.20 |
| Density | Resistivity | Coefficient of Linear Expansion |
| g/cm3 | μΩ•m | a/10-6℃-1 |
| 8.3 | 1.18 | 11.5(20~100℃) |
| Heat Treatment Method | Tensile Strength σb/MPa | Elongation σ5 /% |
| Solution Treatment | 735 | 40 |

Professional Customization
| Cold-drawn Wire | ¢0.3~¢18mm(Delivery in rolls or trays) |
| Hot-Rolling Wire | ¢5.5~¢20mm(Delivery in rolls) |
| Strip | thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips) |
| Smooth Forged Rod on a Lathe | ¢60~350mm,L800-2500mm |
| Hot-rolled Burnishing | ¢20~80mm,L1000-5000mm |
| Cold Drawn and Burnishing | ¢2.5~18mm,L1000-8000mm |
| Seamless Tube | ¢1~275mm,wall thickness 0.2~30,L1000-8000mm |






|