Superalloy Alloy Flat Bar INCONEL 693 With SGS Approval

Categories Alloy Steel Flat Bar
Brand Name: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number: INCONEL alloy693
Certification: SGS,TUV,BV,ISO,MTC
Place of Origin: China
MOQ: Negotiations
Price: Negotiations
Payment Terms: T/T
Supply Ability: 100000KGS/Month
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Packaging Details: Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name: INCONEL alloy693 Alloy Round Bar
Grades: INCONEL alloy693
Processing methods: Shot blasted,Ground,Peeled,Cold working,Machined,etc
Surface: Black,Bright,Rrough Turned,Grinding,Centreless Ground,etc
Profile: Round Bar,Flat Bar,Forging Parts,Sheets Plates,Forging Piece,etc
Price Term: Ex-work,FOB,CIF,CFR, DDU etc.
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Superalloy Alloy Flat Bar INCONEL 693 With SGS Approval

INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 Bar


Description


Our company provides INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 ESR refined Bar INCONEL693 Cold working Bar.

All of INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 ESR refined Bar INCONEL693 Cold working Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.


  • Material:Metal,INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 Bar
  • Shape:Superalloy Flat Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

Products Details


INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 ESR refined Bar INCONEL 693Cold working Bar


Chemical Composition (weight%):Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.15
Si (%): ≤ 0.50
Mn (%): ≤ 1.00
P (%) ≤: 0.030
S (%) ≤: 0.010
Cr (%): 27.0 ~ 31.0
Ni (%): Remainder
Mo (%): -
Cu (%): ≤ 0.50
Al (%): 2.50 ~ 4.00
Ti (%): ≤ 1.00
Nb (%): 0.50 ~ 2.50
Co (%): -
W (%): -
Fe (%): 2.50 ~ 6.00

Condition: Cold/ Hot worked, annealed
Tensile strength, σb/≥ MPa: 690
Yield strength, σ0.2/≥ MPa: 345
Elonghation, δ ≥(%): 30.0


Applications:


INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 ESR refined Bar INCONEL693 Cold working Bar


The alloy is usually produced by AOD / VOD /VIM followed by electroslag refining (ESR) / VAR if necessary for special purpose.
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different levels according to the buyers' requirements.
Bars are usually supplied bright surface in the solution annealed condition.


INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 ESR refined Bar INCONEL 693Cold working Bar


FAQ


Q: How do you control the quality?


A: We have professional inspectors to analyze the chemical composition of INCONEL alloy693 Alloy Steel Flat Bar INCONEL 693 Superalloy Flat Bar INCONEL693 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.



Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc

Quality Superalloy Alloy Flat Bar INCONEL 693 With SGS Approval wholesale
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0